Material Analysis
10 Aufrufe
Fast UV Aging of CMC
Problembeschreibung
After 48h of UV irradiation, CMC mechanical properties decrease by >20% and yellowing occurs
Ursachenanalyse
CMC molecular chains rapidly degrade by photo-oxidation under UV; surface molecular chains break to form microcracks
Lösung
1)Add UV absorber 0.3-0.5wt% to block UV; 2)Add HALS 0.2wt% for radical scavenging; 3)Carbon black 2wt% to physically shield UV
Wichtigste Erkenntnis
Fast UV aging is caused by photo-oxidation; UV absorber and HALS are the key