Injection Molding 4 Aufrufe

DSTDP injection weld line low strength

Problembeschreibung
DSTDP injection multi-gate product strength at the weld line is only 30-40% of the whole
Ursachenanalyse
The temperature of the two melt fronts has dropped, molecular chain diffusion depth small, entanglement insufficient; dispersed phase orientation at the weld line discontinuous
Lösung
1) Raise injection temperature 10-15°C to increase diffusion depth; 2) raise injection speed to keep the front temperature higher; 3) increase holding pressure to ensure the weld is compacted; 4) set an overflow well at the weld line and cut off afterwards
Wichtigste Erkenntnis
Low weld line strength is caused by insufficient molecular entanglement; high-temperature high-speed injection and overflow well are effective countermeasures
DSTDP injectionweld lineinsufficient entanglementinjection temperatureoverflow well