Material Analysis
3 Aufrufe
DSTDP insufficient toughness, brittle fracture
Problembeschreibung
DSTDP product elongation at break <50%, brittle fracture without yielding
Ursachenanalyse
DSTDP molecular weight on the low side, toughness foundation insufficient; excessive crosslinking losing toughness; coarse crystallization, brittleness increased
Lösung
1) Select high molecular weight DSTDP to improve toughness; 2) control crosslinking degree to avoid excess; 3) nucleating agent to refine crystallization and improve toughness
Wichtigste Erkenntnis
Insufficient toughness is caused by low molecular weight and coarse crystallization; selecting high MW is key