DSTDP hardness too low

Problembeschreibung
DSTDP product Shore hardness 5-10 degrees lower than target, soft hand feel
Ursachenanalyse
DSTDP soft nature, hardness low; plasticizer or softener added too much; crystallinity on the low side
Lösung
1) Add rigid filler 5-10wt% to increase hardness; 2) reduce plasticizer dosage; 3) increase cooling rate to increase crystallinity
Wichtigste Erkenntnis
Low hardness is caused by material softness and excessive plasticization; adding filler is key
DSTDPhardness too lowrigid fillerplasticizercrystallization control