Injection Molding 4 Aufrufe

Glass Fibre wall thickness too thick

Problembeschreibung
Glass Fibre product wall thickness is 10-15% thicker than the design value
Ursachenanalyse
holding pressure too high, excessive compaction; injection amount too much, overflowing into thick-wall regions; gate too large, holding pressure excessively transmitted
Lösung
1) reduce holding pressure to a moderate level; 2) precisely control injection amount; 3) reduce gate size to limit holding pressure transmission
Wichtigste Erkenntnis
excessive wall thickness is caused by excessive holding; precisely controlling injection amount and holding is key
Glass Fibre wall thickness too thick holding pressure injection amount gate size

War das hilfreich?

0 Personen fanden dies hilfreich

ChemAI