Glass Fibre severe excessive orientation
Problembeschreibung
Glass Fibre products have longitudinal-transverse property difference >50%, excessive orientation
Ursachenanalyse
injection speed too fast, molecular chains highly oriented in the flow direction; gate design causes unidirectional flow
Lösung
1) reduce injection speed to reduce orientation; 2) multi-point gates to reduce unidirectional flow; 3) annealing to partially release orientation
Wichtigste Erkenntnis
excessive orientation is caused by fast unidirectional flow; reducing speed and multi-point gates are key