MP internal coarse crystallization

Problembeschreibung
MP products have internal spherulites >50μm, coarse, causing reduced transparency and low impact
Ursachenanalyse
cooling rate too slow <5°C/min, allowing spherulites to fully grow; no nucleating agent used to control crystallization
Lösung
1) increase cooling rate to >20°C/min to refine spherulites; 2) add 0.2-0.3wt% nucleating agent to control crystallization; 3) lower mold temperature to accelerate cooling
Wichtigste Erkenntnis
coarse crystallization is caused by slow cooling; fast cooling and nucleating agent are key