MP fast UV aging
Problembeschreibung
MP after 48h UV irradiation, mechanical properties decline >20%, yellowing
Ursachenanalyse
MP molecular chains rapidly degrade by photo-oxidation under UV; surface molecular chains break forming microcracks
Lösung
1) add UV absorber 0.3-0.5wt% to block UV; 2) add HALS 0.2wt% for radical scavenging; 3) carbon black 2wt% to physically shield UV
Wichtigste Erkenntnis
fast UV aging is caused by photo-oxidation; UV absorber and HALS are key