PBN mold carbon buildup Problem in Injection Processing
Problembeschreibung
Polybutylene naphthalate PBN exhibits mold carbon buildup in injection processing at 270-300°C.
Ursachenanalyse
Under high-temperature processing at 270-300°C, oxidation causes the problem.
Lösung
Solve by optimizing the mold temperature.
Wichtigste Erkenntnis
PBN ultra-high-temperature processing requires comprehensive protection.