Molding Process
6 Aufrufe
PBN bubble problem in sheet processing
Problembeschreibung
Polybutylene naphthalate PBN shows bubble in sheet processing at 270-300°C.
Ursachenanalyse
Degradation under high-temperature processing at 270-300°C triggers the problem.
Lösung
Solved by precise temperature control.
Wichtigste Erkenntnis
PBN ultra-high-temperature processing requires comprehensive protection.
War das hilfreich?
0 Personen fanden dies hilfreich