Molding Process
6 Aufrufe
PBN flow mark problem in sheet processing
Problembeschreibung
Polybutylene naphthalate PBN shows flow mark in sheet processing at 270-300°C.
Ursachenanalyse
Oxidation under high-temperature processing at 270-300°C triggers the problem.
Lösung
Solved by nitrogen protection.
Wichtigste Erkenntnis
PBN ultra-high-temperature processing requires comprehensive protection.