The heat sealability decrease problem of the easy-tear masterbatch in the PE film
Problembeschreibung
After the easy-tear masterbatch is added to the PE film, heat sealability decrease appears.
Ursachenanalyse
The dispersion uniformity of the easy-tear agent affects the tear characteristics.
Lösung
Improve the dispersion process.
Wichtigste Erkenntnis
The easy-tear masterbatch must take into account both the tear direction and the mechanical balance.