Material Analysis 10 Aufrufe

Problem of poor dispersion of high-temperature resistant masterbatch in PET applications

Problembeschreibung
High-temperature resistant masterbatch shows poor dispersion during high-temperature processing of PET.
Ursachenanalyse
Improper temperature resistance grade of carrier resin.
Lösung
Solve by selecting a high temperature resistant carrier resin.
Wichtigste Erkenntnis
The key of high-temperature resistant masterbatch lies in carrier resin matching.
high-temperature resistant masterbatchpoor dispersionPETcarrier resintemperature resistance