Regulation of sharkskin of PPA in sheet Processing
Problembeschreibung
The sharkskin abnormality of the PPA processing aid in sheet production affects efficiency.
Ursachenanalyse
The sharkskin of the PPA fluoropolymer is unsatisfactory at an addition amount of 0.02%, and the addition method needs to be optimized.
Lösung
Adjust the PPA addition amount combined with screw design.
Wichtigste Erkenntnis
The key to the performance of PPA lies in uniform dispersion.