Production & Quality
3 Aufrufe
PPS regrind degradation
Problembeschreibung
PPS recycled material oxidatively crosslinks after multiple regranulation and becomes unusable.
Ursachenanalyse
During multiple high-temperature processing, PPS gradually oxidatively crosslinks, turning black and brittle.
Lösung
Limit reuse times to 1-2; do not set recycling granulation temperature too high.
Wichtigste Erkenntnis
Use of PPS recycled material requires great caution.