Processing Machinery 3 Aufrufe

PPSU barrel cleaning extremely difficult

Problembeschreibung
PPSU high-temperature residual material carbonizes and is difficult to remove from the barrel.
Ursachenanalyse
At 380°C, residual PPSU carbonizes and forms a carbon layer that is difficult to remove.
Lösung
Use professional high-temperature purging compound; replace with low-melting plastic before shutdown.
Wichtigste Erkenntnis
PPSU cleaning is a high-risk operation.
PPSUcleaningcarbonizationhigh temperaturereplacement