Molding Process 6 Aufrufe

POE internal coarse crystallization

Problembeschreibung
POE product internal spherulites >50μm coarse, causing transparency drop and low impact
Ursachenanalyse
Cooling rate too slow <5°C/min allows spherulites to fully grow; no nucleating agent used to control crystallization
Lösung
1) Increase cooling rate to >20°C/min to refine spherulites; 2) Add 0.2-0.3wt% nucleating agent to control crystallization; 3) Lower mold temperature to accelerate cooling
Wichtigste Erkenntnis
Coarse crystallization is caused by slow cooling; fast cooling and nucleating agent are key
POEcoarse crystallizationspherulite refinementnucleating agentcooling rate