POE toughened PP hardness greatly reduced

Problembeschreibung
POE/PP Shore D drops from 65 to 40, below 50
Ursachenanalyse
POE soft, D<30, drops greatly after adding 15-20wt%
Lösung
1) POE reduced to 8-12wt%; 2) Talc 10-15wt% compensation; 3) PP/POE/talc ternary; 4) POE+nucleating agent to reduce hardness loss
Wichtigste Erkenntnis
Toughening is accompanied by hardness drop, requiring filler compensation
POE toughened PPhardness dropfiller compensationternary compositenucleating agent