Material Analysis
6 Aufrufe
POE surface blooming exudation
Problembeschreibung
POE product surface exudes white frost-like low molecular substances, affecting appearance
Ursachenanalyse
Low molecular weight components in POE migrate to the surface and exude during storage; lubricant or plasticizer supersaturated exudation
Lösung
1) Select high molecular weight POE to reduce low molecular substances; 2) Reduce lubricant addition to a reasonable level; 3) Clean product surface and then detect the source
Wichtigste Erkenntnis
Blooming is caused by low molecular migration and exudation; selecting high molecular weight grade is fundamental
War das hilfreich?
0 Personen fanden dies hilfreich