Material Analysis
3 Aufrufe
POE elongation at break low
Problembeschreibung
POE product elongation at break <100%, below 200% requirement
Ursachenanalyse
POE molecular weight low, chains short, entanglement insufficient; excessive orientation, transverse elongation extremely low; excessive crosslinking restricts chain slippage
Lösung
1) Select high molecular weight POE to increase entanglement density; 2) Reduce orientation, lower injection speed; 3) Control crosslinking degree to avoid excess
Wichtigste Erkenntnis
Low elongation at break is caused by low molecular weight and orientation; selecting high MW and reducing orientation are key