Production & Quality
3 Aufrufe
TPO poor dimensional stability
Problembeschreibung
Product dimensions gradually change during storage
Ursachenanalyse
Internal stress slowly released post-shrinkage post-crystallization
Lösung
Full annealing optimize process reduce residual stress
Wichtigste Erkenntnis
Dimensional stability core of precision products
War das hilfreich?
0 Personen fanden dies hilfreich