Processing Machinery
6 Aufrufe
TPU melt residence time in the barrel too long
Problembeschreibung
The product color darkens, degradation appears
Ursachenanalyse
Continuous production is interrupted, the material in the barrel is heated for a long time
Lösung
Empty the barrel after 10 minutes of shutdown, plan reasonably to reduce shutdowns
Wichtigste Erkenntnis
Reducing the residence time is a basic principle
War das hilfreich?
0 Personen fanden dies hilfreich