Processing Machinery 2 Aufrufe

Black spots/discoloration appearing on FEP products

Problembeschreibung
FEP products become darker in color or show black spots
Ursachenanalyse
Improper processing temperature control causes overheating and decomposition; material stagnates in the equipment
Lösung
Precisely control the temperature ≤380°C; shorten the residence time
Wichtigste Erkenntnis
The decomposition of FEP is irreversible
black spotsdecompositionresidence timeFEP

War das hilfreich?

0 Personen fanden dies hilfreich

ChemAI