Filling difficulty of PVDF long-flow products

Problembeschreibung
The far end of large thin-walled products is not fully filled
Ursachenanalyse
The melt flow path is long, the pressure decay is large, and the front edge cools
Lösung
Multi-gate arrangement, raise the melt temperature, and increase the injection speed
Wichtigste Erkenntnis
Gate layout is the key
PVDFfilling difficulty