Processing Machinery
3 Aufrufe
Linear low-density polyethylene pipe failing pressure test
Problembeschreibung
The pipe ruptures or leaks in the hydraulic test, and pressure resistance does not meet standards.
Failing the pressure test directly threatens the safety of pipe use and is a fatal defect in water supply and gas pipelines.
Ursachenanalyse
(1) Pipe wall thickness is insufficient or uneven
(2) Material degradation causes molecular weight reduction
(3) There are bubbles or impurities inside the pipe
(4) Inappropriate crystallinity results in poor mechanical properties
(5) Insufficient melt plasticization results in poor welding
Lösung
(1) Check and adjust pipe wall thickness to ensure uniform wall thickness at all parts meets standards
(2) Control extrusion temperature within the 190-250°C range to avoid material degradation
(3) Fully dry the raw material to ensure it is clean
(4) Optimize cooling conditions to ensure appropriate crystallinity of linear low-density polyethylene
(5) Optimize screw design to ensure full plasticization
Wichtigste Erkenntnis
Pressure test failure is caused by insufficient wall thickness, material degradation or internal defects and needs to be systematically solved from process and material quality.
War das hilfreich?
0 Personen fanden dies hilfreich
Vielen Dank für Ihr Feedback!