Yellowing of PAR '2079851475616104452 due to improper temperature control
Problembeschreibung
The color of PAR products turns yellow and the transparency decreases.
Ursachenanalyse
The processing temperature is too high >320°C or the residence time is long, causing thermal oxidative degradation, and the aromatic structure oxidizes and turns yellow.
Lösung
Strictly control the processing temperature at 280-310°C, not exceeding 320°C; shorten the residence time; add antioxidants when necessary.
Wichtigste Erkenntnis
Although PAR has good thermal stability, strict temperature control is still required.