Material Analysis 10 Aufrufe

Internal stress detection of PAR products

Problembeschreibung
The internal stress detection method (solvent method) is time-consuming.
Ursachenanalyse
The polarizer method is semi-quantitative, and the solvent method for full inspection is too slow.
Lösung
Combine rapid polarizer screening and solvent method sampling.
Wichtigste Erkenntnis
PAR stress detection efficiency needs to be optimized.
PARstresspolarizersolvent