Injection Molding 10 Aufrufe

Translucent/Hazy PBT Injection-Molded Parts (Non-Transparent Grade)

Problembeschreibung
Partially translucent or hazy areas appear in natural-color non-transparent PBT products.
Ursachenanalyse
The local area is not fully crystallized (rapid cooling causes incomplete crystallization), and the optical properties of this area are different from those of the fully crystallized area.
Lösung
Increase the mold temperature to ensure uniform crystallization; extend the cooling time; anneal the product to homogenize crystallization.
Wichtigste Erkenntnis
PBT haziness is the optical manifestation of uneven crystallization.
PBThazecrystallizationannealing