Excessively Long PBT '2079851475616104452 Cycle
Problembeschreibung
The PBT '2079851475616104452 cycle exceeds the industry average level for similar products.
Ursachenanalyse
The cooling time is too long (affected by the product wall thickness and mold cooling efficiency); the melt temperature is too high, requiring a longer cooling time.
Lösung
Optimize the cooling water channels to improve efficiency; appropriately reduce the mold temperature; adjust the melt temperature.
Wichtigste Erkenntnis
PBT molding cycle optimization is the key to improving production efficiency.