Fiber Residue of PBT Reinforced Material After Incineration
Problembeschreibung
After PBT products are incinerated or decomposed at high temperature, a glass fiber skeleton remains.
Ursachenanalyse
During end-of-life treatment of the product, the PBT matrix resin decomposes but the glass fiber remains, affecting recycling or incineration.
Lösung
Design a recyclable solution (mechanical recycling first); communicate the disposal plan with end customers.
Wichtigste Erkenntnis
Attention needs to be paid to environmental protection in the disposal of PBT glass fiber reinforced material.