Injection Molding
10 Aufrufe
Insufficient Actual Weight in PBT '2079851475616104452
Problembeschreibung
The actual weight of the product is less than the theoretical weight (insufficient density).
Ursachenanalyse
The holding is insufficient and the product is not dense enough; the injection amount is insufficient; the material degrades and the density decreases.
Lösung
Increase the holding pressure and extend the time; ensure the injection amount is sufficient; reduce the processing temperature.
Wichtigste Erkenntnis
PBT weight is an intuitive indicator of product quality.
War das hilfreich?
0 Personen fanden dies hilfreich