Material Analysis 10 Aufrufe

Poor weather resistance and yellowing of PET products

Problembeschreibung
PET products severely yellow after 6-12 months of outdoor use, and mechanical properties decline.
Ursachenanalyse
PET is sensitive to ultraviolet (UV) radiation; UV radiation causes photo-oxidative degradation; insufficient light stabilizer is added to the product.
Lösung
Add UV absorbers (benzotriazole type) and HALS; use TiO2 ultraviolet screening agents; apply surface UV protective coatings.
Wichtigste Erkenntnis
PET outdoor applications must undergo light stabilization treatment.
PETweather resistanceyellowingultravioletlight stabilizer