Problembeschreibung
After hot filling and cooling, the body of the PET hot-fill bottle dents inward and deforms, and the label wrinkles.
Ursachenanalyse
Hot filling and cooling produce negative pressure; the bottle structure strength is insufficient to resist the negative pressure; bottle body reinforcing rib design is insufficient; wall thickness is inadequate.
Lösung
Adopt hot-fill special bottle designs (adding vacuum absorption panels); increase wall thickness; use heat-resistant PET grades; use nitrogen filling compensation.
Wichtigste Erkenntnis
PET hot-fill bottles need special structural design and material selection to cope with negative pressure.