Injection Molding 3 Aufrufe

Fluidity decline of PET modified material

Problembeschreibung
After adding fillers (glass fiber, mineral powder) or flame retardants to PET, MFI decreases significantly and '2079851475616104452 is difficult.
Ursachenanalyse
Rigid fillers increase melt viscosity (particle-particle and particle-molecular chain friction); fillers are not surface-treated.
Lösung
Use silane coupling agents to treat fillers; control filler dosage and particle size distribution; add lubricants or flow modifiers.
Wichtigste Erkenntnis
The fluidity loss of PET filled modification needs to be compensated through filler surface treatment and process adjustment.