Injection Molding
3 Aufrufe
PETG injection mold parting line overflow
Problembeschreibung
PETG melt overflows at the mold parting line, and the product has flash.
Ursachenanalyse
Clamping force insufficient or unevenly distributed, parting line worn and uneven, injection pressure high.
Lösung
Increase and evenly distribute the clamping force; repair the parting line flatness; appropriately reduce injection pressure and speed.
Wichtigste Erkenntnis
PETG overflow is a mold closing and mold precision problem.
War das hilfreich?
0 Personen fanden dies hilfreich
Vielen Dank für Ihr Feedback!