Injection Molding 3 Aufrufe

Improper barrel temperature setting of PLA '2079851475616104452 causing degradation

Problembeschreibung
The barrel temperature is too high, causing PLA degradation and yellowing.
Ursachenanalyse
PLA has poor thermal stability; the temperature of each section is set too high, and it degrades rapidly above 200-220°C.
Lösung
Set according to a decreasing curve: rear section 160-170°C, middle section 175-185°C, front section 180-190°C.
Wichtigste Erkenntnis
The PLA barrel temperature setting should be conservative.
PLA barrel temperature degradation temperature curve