Injection Molding 3 Aufrufe

Long PLA '2079851475616104452 cycle (slow cooling)

Problembeschreibung
The PLA '2079851475616104452 cycle is too long, affecting production capacity.
Ursachenanalyse
PLA releases heat during cooling crystallization and has a low thermal conductivity, so it cools slowly; the crystalline type needs a longer time.
Lösung
Optimize the mold cooling design; lower the melt temperature; use amorphous PLA to shorten the cycle.
Wichtigste Erkenntnis
The slow cooling of PLA is a constraint on production efficiency.
PLA cooling cycle crystallization thermal conductivity