Material Analysis
10 Aufrufe
Large molecular weight decrease after PLA mechanical recycling
Problembeschreibung
After mechanical recycling, the intrinsic viscosity of PLA decreases by >20%.
Ursachenanalyse
The combination of thermal and mechanical degradation causes molecular chain breakage and a large decrease in molecular weight.
Lösung
Reduce the recycling processing temperature; add a chain extender to restore the molecular weight.
Wichtigste Erkenntnis
The molecular weight decay of PLA recycling is a reuse challenge.