Injection Molding
6 Aufrufe
Insufficient filling of PMMA '2079851475616104452
Problembeschreibung
The cavity is not completely filled.
Ursachenanalyse
PMMA melt viscosity is high, injection pressure and speed are insufficient, and mold temperature is low, so the melt solidifies prematurely.
Lösung
Increase melt temperature to 220-250°C; increase injection pressure and speed; mold temperature 60-90°C.
Wichtigste Erkenntnis
PMMA fluidity is the main cause of '2079851475616104452 short shot.