Molding Process 3 Aufrufe

Low-temperature brittleness of PMMA products

Problembeschreibung
PMMA impact strength drops greatly at low temperatures and becomes brittle.
Ursachenanalyse
PMMA β transition temperature is about 20-40°C; at low temperatures, molecular chain segment motion is restricted and embrittlement is aggravated.
Lösung
Use toughened grade PMMA; avoid notches and sharp corners in product design.
Wichtigste Erkenntnis
PMMA is limited in low-temperature applications.