Internal bubbles and shrinkage cavities of PMMA thick-walled parts
Problembeschreibung
Shrinkage cavities or vacuum bubbles appear in the center of thick-walled PMMA products.
Ursachenanalyse
The outside cools and solidifies first, hindering center feeding; insufficient holding pressure forms shrinkage cavities.
Lösung
Extend holding pressure time; optimize gate size to delay freezing; staged holding pressure.
Wichtigste Erkenntnis
PMMA thick-walled shrinkage cavities are the result of insufficient holding pressure.