Surface mold deposit of POM injection molded products
Problembeschreibung
After a period of POM '2079851475616104452, white film-like mold deposit appears on the mold.
Ursachenanalyse
Formaldehyde, oligomeric formaldehyde and additives released from POM decomposition deposit on the mold surface.
Lösung
Regularly clean the mold; reduce processing temperature; add stabilizer.