Chemical Resistance of polyamide 6 (nylon 6) Changed After Modification

Problembeschreibung
The chemical resistance of polyamide 6 (nylon 6) changes after modification, with the resistance to specific chemicals decreasing or increasing
Ursachenanalyse
The added additives change the chemical structure of the material The toughening agent reduces the chemical resistance The flame retardant may increase the chemical resistance The interaction of the components in the formulation is complex The matrix characteristics of polyamide 6 (nylon 6) change
Lösung
Evaluate the change in chemical resistance after modification Select a toughening agent that does not affect chemical resistance Utilize the chemical resistance improvement of the flame retardant Comprehensively consider the influence of each component of the formulation Maintain the matrix characteristics
Wichtigste Erkenntnis
The chemical resistance needs to evaluate the overall influence of the modified formulation
chemical resistanceformulationtoughening agentflame retardant