Material Analysis
7 Aufrufe
LGFPP recycled material performance degradation
Problembeschreibung
After adding 30% recycled material, product performance declines by more than 40%
Ursachenanalyse
The glass fiber length in the recycled material is only below 30% of the original length; multiple thermal histories break the chemical bonds at the PP-glass fiber interface; the PP matrix itself degrades and the molecular weight decreases
Lösung
Strictly control the recycled material addition ratio ≤20-30%; fully premix recycled material with virgin material; use recycled material preferentially for non-critical structural parts
Wichtigste Erkenntnis
Multiple thermal histories of LGFPP cause irreversible performance degradation
War das hilfreich?
0 Personen fanden dies hilfreich