Processing Machinery
3 Aufrufe
PAEK high-temperature degradation producing black spots
Problembeschreibung
Black spots and burnt odor appear on the product
Ursachenanalyse
Processing temperature exceeds 400°C; the material stays in the barrel too long
Lösung
Strictly control temperature ≤400°C; shorten residence time to ≤5 minutes
Wichtigste Erkenntnis
PAEK thermal degradation is as irreversible as PEEK
War das hilfreich?
0 Personen fanden dies hilfreich