PAEK thermo-oxidation at high temperature
Problembeschreibung
After long-term high-temperature use, the mechanical properties of PAEK decline significantly
Ursachenanalyse
At high temperature, the molecular chains of PAEK undergo oxidative scission; the stabilizer is consumed
Lösung
Evaluate the long-term use temperature upper limit of the specific PAEK grade; reserve a safety margin in design
Wichtigste Erkenntnis
PAEK long-term heat resistance requires evaluation of thermo-oxidative stability