Praktische Antworten auf häufige Herausforderungen mit Kunststoffmaterialien

1506 Fragen
Q
Poor hot runner balance in PET '2079851475616104452
Q
Warpage deformation of PET injection molded parts
A
The root of PET warpage lies in uneven shrinkage.
Injection Molding PETwarpagedeformationuneven shrinkageproduct design
Q
Scaling in PET mold cooling water channels
Q
Insufficient filling/short shot in PET preform injection
A
PET preform short shot is usually related to excessive flow resistance.
Injection Molding PETshort shotinsufficient fillinginjection pressuregate
Q
Insufficient weld line strength of PET injection molded parts
A
PET weld line strength needs to be comprehensively improved through temperature, pressure and gate layout.
Injection Molding PETweld lineinsufficient strengthmolecular chain orientationventing
Q
Fiber exposure in PET reinforced material
A
The surface quality of PET reinforced products depends on high-temperature molds and fast filling.
Injection Molding PETglass fiber exposuremold temperatureinjection speed
Q
Gate blush in PET '2079851475616104452
Q
Nozzle drooling in PET '2079851475616104452
A
PET nozzle drooling affects production stability.
Injection Molding PETnozzle droolingdrippingshut-off nozzleback pressure
Q
Radial streaks on the surface of PET products
A
PET radial streaks are caused by unstable melt front flow.
Injection Molding PETradial streaksmelt frontinjection speed
Q
Whitening in the gate area of PET preforms