Q
Glass Fibre '2079851475616104452 severe flash
A
Flash is caused by high-pressure injection and mold gap; reducing pressure and improving mold fit are key
Injection Molding Glass Fibre injectionflashclamping forceparting lineinjection pressure
Q
Glass Fibre injection molded product has oil spots
Q
Glass Fibre '2079851475616104452 insufficient flow length ratio
A
Insufficient flow length ratio is caused by Glass Fibre high viscosity; high temperature, high pressure and large gate are key
Injection Molding Glass Fibre injectionflow length ratiomelt viscosityinjection temperatureflow aid
Q
Glass fiber reinforced plastic severe floating fiber
A
Floating fiber is caused by poor interface and injection orientation; coupling agent and reduced injection speed are key
Injection Molding glass fiber floating fibercoupling agentMAH compatibilizerinjection speedglass fiber length
Q
Glass Fibre injection gate freezes too early
A
Premature gate freezing is caused by small gate and low temperature; enlarging gate and raising temperature are fundamental measures
Injection Molding Glass Fibre injectiongate freezingholding pressure transmissiongate sizemold temperature
Q
Glass Fibre injection mold venting burnt
A
Q
Glass Fibre mixed with color masterbatch uneven color
A
Color masterbatch carrier matching and full dispersion are the key to color uniformity
Injection Molding Glass Fibre coloringcolor masterbatchcarrier compatibilitypigment dispersioncolor streaks
Q
Glass Fibre '2079851475616104452 warpage deformation
A
Warpage is caused by shrinkage differences and orientation stress; uniform mold temperature and holding pressure are key
Injection Molding Glass Fibre injectionwarpageshrinkage rateholding pressureannealing treatment
Q
Glass Fibre '2079851475616104452 difficult demolding
A
Difficult demolding is caused by adhesion and insufficient mold design; increasing draft angle is the fundamental measure
Injection Molding Glass Fibre injectiondifficult demoldingdraft angleadhesionejection design
Q
DSTDP periodic surface ripples
A
Ripples are caused by unstable injection; equipment overhaul and PID control are key