Injection Molding 4 Aufrufe

DSTDP periodic surface ripples

Problembeschreibung
DSTDP product surface periodic ripples, spacing 5-15mm
Ursachenanalyse
Injection speed periodically fluctuates; hydraulic system unstable; screw speed unstable
Lösung
1) Overhaul injection system to stabilize pressure and speed; 2) servo motor drive instead of hydraulic drive; 3) PID control to stabilize injection parameters
Wichtigste Erkenntnis
Ripples are caused by unstable injection; equipment overhaul and PID control are key
DSTDPsurface ripplesinjection stabilityequipment overhaulPID control

War das hilfreich?

0 Personen fanden dies hilfreich