DSTDP periodic surface ripples
Fenómeno del problema
DSTDP product surface periodic ripples, spacing 5-15mm
Análisis de la causa
Injection speed periodically fluctuates; hydraulic system unstable; screw speed unstable
Solución
1) Overhaul injection system to stabilize pressure and speed; 2) servo motor drive instead of hydraulic drive; 3) PID control to stabilize injection parameters
Conclusión clave
Ripples are caused by unstable injection; equipment overhaul and PID control are key